Home | Shop | PCB40 Cement

PCB40 Cement

Outstanding features:

  • High compressive strength
  • Stable, R28>45MPa
  • Complies with TCVN 6260:2020
  • Good adhesion
  • Waterproof, anti-cracking, sulfate resistant
  • Application: Concrete, columns, beams, waterproofing
  • Large load-bearing structures: bridges, ports, hydroelectric dams
Liên hệ đặt hàng Tư vấn kỹ thuật

Outstanding features: High compressive strength; stable, R28>45MPa in accordance with TCVN 6260:2020; good adhesion; waterproof, crack-resistant, sulfate-resistant; Application: Concrete, columns, beams, waterproofing; Large load-bearing structures: bridges, ports, hydroelectric dams.

Test results:

No.TEST ITEM
(Items)
UNIT
(Units)
TEST METHOD
(Test Method)
SPECIFICATION
(Spec. limit)
TEST RESULT
(Test Results)
1COMPRESSIVE STRENGTH

  • After 3 days ± 45 min
  • After 28 days ± 8 h
N/mm²
N/mm²
TCVN 6016:2011≥18
≥40
31.5
44.0
2TIME OF SETTING:

  • Initial set
  • Final set
Minutes
Minutes
TCVN 6017:2015≥45
≤420
155
235
3FINENESS TEST

  • Residue on 0.09 mm sieve
  • Residue on 0.045 mm sieve
  • Specific surface area (Blaine method)
%
%
cm²/g
TCVN 13605:2003

≥ 2,800
1.55
12.5
4,050
4SOUNDNESS (Le Chatelier method)mmTCVN 6017:2015≤101.00
5CHEMICAL COMPOSITION
Sulfur trioxide content (SO₃), max%TCVN 141:2023≤3.51.85
Loss on ignition (LOI), max%TCVN 141:2023≤106.01
6AUTOCLAVE EXPANSION, max%TCVN 8877:20110.80.04

STORAGE

  • The warehouse floor must be high and dry
  • Do not stack directly on the floor, do not stack more than 10 bags on top of each other and place at least 20cm away from the wall

NOTE DURING USE

  • Sand, stone, water must be clean, not salty, dry mix well before mixing with water
  • Use up all the stone mixture within 2 hours, when pouring concrete, compact it firmly
  • Cover from rain for the first 10 hours, moisturize for the first 20 days
  • If using aggregates with specifications different from the above instructions, please contact the dealer for exact usage